1.1 ,This practice covers procedures for preparing and conducting the polythionic acid test at room temperature, 22 to 25°,C (72 to 77°,F), to determine the relative susceptibility of stainless steels or other related materials (nickel-chromiumiron alloys) to intergranular stress corrosion cracking.